【文章摘要】 Pyrolusite reduction processes by three major biomass components cellulose,hemicelluloses and lignin,represented by CP,HP and LP,respectively,were investigated by thermogravimetric analyzer coupled with Fourier transform infrared spectrometry(TG-FTIR).The Sestak-Berggren(SB) equation was used to evaluate the kinetics of reduction processes.TG analysis reveals that the main reduction processes occur at 250-410 ℃,220-390 ℃,and 190-410 ℃ for CP,HP,and LP,respectively.FT-IR and XRD results indicate that various reducing volatiles(e.g.aldehydes,furans,ketones and alcohols) are produced from the pyrolysis with the three major components,which directly reduce MnO_2 in ore to MnO.The processes are described by the SB equation with three parameters(m,n,p).Their non-zero values suggest that pyrolusite reduction is controlled by the diffusion of reducing gaseous products through an ash/inert layer associated with minerals.The apparent activation energies for pyrolusite reduction by CP,HP and LP are 40.48,25.70 and 40.10 kJ·mol~(-1),respectively. |